Résumé
Applicable to products having contents of AlF3 of more than 0.15 % (m/m) or of NaF of more than 0.4 % (m/m). Covers sintering of a test portion with a known quantity of sodium fluoride in a muffle furnace at a temperature of (790 10) °C. Under these conditions, aluminium fluoride in excess of that required by the stoichiometric formula AlF3 .3NaF reacts to form cryolite; extraction of the ground sintered mass with boiling water. Acidification with hydrochloric acid solution to a pH less than 3.7 and titration of the excess sodium fluoride with thorium nitrate solution in the presence of alizarin-S as indicator. Has also been approved by the IUPAC.
Informations générales
-
État actuel: AnnuléeDate de publication: 1977-11Stade: Annulation de la Norme internationale [95.99]
-
Edition: 1Nombre de pages: 3
-
Comité technique :ISO/TC 226ICS :71.060.50