Resumen
A test portion is deated in a tared platinum crucible, in a furnace at 700 degrees centigrade, under oxidizing and specified conditions, to constant mass. The residue is cooles and weighed. The method is applicable to products (tar pitch, petroleum pitch, etc.) producing a quality of ash greater than or equal to 0,05 % (m/m).
Preview
Previsualice esta norma en nuestra Plataforma de navegación en línea (OBP)
Informaciones generales
-
Estado: PublicadoFecha de publicación: 1985-09Etapa: Norma Internacional confirmada [90.93]
-
Edición: 1Número de páginas: 3
-
Comité Técnico :ISO/TC 226ICS :71.100.10