Тезис
ПредпросмотрThis document describes two methods for measuring stress in tension under non-isothermal conditions.
— Method A: The thermal stress is measured for various pre-strain and temperature conditions as a function of time.
— Method B: The change of stress is measured in a test piece at a given strain and under variation of temperature at a given heating rate as a function of temperature. In this way, the determination of the thermal-mechanical behaviour of a rubber can be accelerated, e.g. for the purpose of comparative testing of aging or estimating the upper limit of the operating temperature.
The measurement device, which is equipped with a suitable heating chamber, is used to record the stress as a function of time or temperature until the sample breaks or the stress has approached zero or for a certain time.
-
Текущий статус: PublishedДата публикации: 2023-01
-
Версия: 3
-
- ICS :
- 83.060 Rubber
Приобрести данный стандарт
Формат | Язык | |
---|---|---|
std 1 92 | PDF + ePub | |
std 2 92 | Бумажный |
- CHF92
Жизненный цикл
-
Ранее
WithdrawnISO 12493:2017
-
Сейчас
-
00
Предварительная стадия
-
10
Стадия, связанная с внесением предложения
-
20
Подготовительная стадия
-
30
Стадия, связанная с подготовкой проекта комитета
-
40
Стадия, связанная с рассмотрением проекта международного стандарта
-
50
Стадия, на которой осуществляется принятие стандарта
-
60
Стадия, на которой осуществляется публикация
-
90
Стадия пересмотра
-
95
Стадия, на которой осуществляется отмена стандарта
-
00
Появились вопросы?
Ознакомьтесь с FAQ
Часы работы:
Понедельник – пятница: 09:00-12:00, 14:00-17:00 (UTC+1)
Будьте в курсе актуальных новостей ИСО
Подписывайтесь на наши новости, обзоры, а также на информацию о продуктах.