ISO/AWI 2507-1
u
ISO/AWI 2507-1
85780

Résumé

The method specified is based on determining the temperature at which a standard indenter, under a force of 50 N ± 1 N, penetrates 1 mm into the surface of a test piece cut from the wall of a pipe or fitting while the temperature is raised at a constant rate. Is applicable only to thermoplastics materials for which it is possible to measure the temperature at which the rate of softening becomes rapid. Is based on ISO 306:1994 which, however, applies to materials in the form of sheets.


Informations générales 

  •  :  Projet
  •  : 2
  •  : ISO/TC 138/SC 5 Propriétés générales des tubes, raccords et robinetteries en matières plastiques et leurs accessoires -- Méthodes d'essais et spécifications de base
  •  :

Vous avez une question?

Consulter notre FAQ

Service à la clientèle
+41 22 749 08 88

Horaires d’ouverture:
De lundi à vendredi - 09:00-12:00, 14:00-17:00 (UTC+1)

Suivez l'actualité de l'ISO

Inscrivez-vous à notre Newsletter (en anglais) pour suivre nos actualités, points de vue et informations sur nos produits.